Safety glass tempered glass curtain wall of glass, wired glass, hollow glass, wire glass should be customized according to the design in the factory, does not allow cutting, punching, dig holes for the installation site.
Glass edge processing should be conducted (chamfering, chamfer, grinding), stress concentration and to prevent rupture.
Gel plates should be on a static site can be replaced after maintenance. Two-component structural adhesive should rest for 3 days, one-component structural adhesive stand for 7 days before shipping. Brought on to the site within the room, continue to 14-21 days, to installation.
Weather resistant adhesive sealing thickness should be not less than 3.5mm, width not less than 7mm. Avoiding three-sided paste on paste, no adhesive tape should be placed on the material at the bottom and then glue to prevent gel break, causing permeability

Glass edge processing should be conducted (chamfering, chamfer, grinding), stress concentration and to prevent rupture.
Gel plates should be on a static site can be replaced after maintenance. Two-component structural adhesive should rest for 3 days, one-component structural adhesive stand for 7 days before shipping. Brought on to the site within the room, continue to 14-21 days, to installation.
Weather resistant adhesive sealing thickness should be not less than 3.5mm, width not less than 7mm. Avoiding three-sided paste on paste, no adhesive tape should be placed on the material at the bottom and then glue to prevent gel break, causing permeability